The Alkaline Paper Advocate

Volume 1, Number 4
Oct 1988


Publishers

British publishers use much acidic paper.

Singapore (World Scientific Publishing Co.) ditto.

European printed books are much more likely to be acidic than those printed here.

A couple of books a month, say 1/2%., declare use of alkaline paper but test acid, < 6.0 with chlorophenol red.