These are all fine paper mills, in the sense that they make at least some coated or uncoated freesheet used for printing or writing. Some of the mills also make other kinds of paper. The production figure (tons per day) reflects all kinds of papers made at the mill. In some cases, the production for individual mills is unavailable. In other cases, it is lumped together for all mills within the many located in that town. Mills that are not completely converted (i.e., that make some acidic fine paper) are not listed.

Company & Location Tons/day

Boise Cascade, Jackson, AL

240

Boise Cascade, Wallula, WA

590

Byron Weston, Dalton, MA

70

Consolidated, Wisconsin Rapids, WI (3 mills)

680

Crane, Dalton, MA (3 mills)

120

Eastern, Brewer, ME

180

Ecusta, Pisgah Forest, NC

300

Finch, Pruyn; Glens Falls, NY

575

Fletcher, Alpena, MI

85

Glatfelter, Neenah, WI

380

Glatfelter, Spring Grove, PA

800

Grays Harbor, Hoquiam, WA

375

Hammermill, Erie, PA

550

Hammermill, Lock Haven, PA

725

Hammermill, Selma, AL

525

International Paper, Mobile, AL

1000

International Paper, Ticonderoga, NY

690

James River, Groveton, NH

300

Mead, Chillicothe, OH (1 of the 3 mills there)

400

Miami, West Carrollton, OH

300

Miller's Falls, Millers Fall, MA

50

Mohawk, Cohoes, NY

120

Mohawk, Waterford, NY

110

Nekoosa, Nekoosa, WI

575

NVF, Parsons Paper Div., Holyoke, MA

35

Papyrus Newton Falls, Newton Falls, NY

400

Potlatch/Northwest, Brainerd, MN

45

Potlatch/Northwest, Cloquet, MN

550

Potsdam, Potsdam, NY

 

Simpson Plainwell, Plainwell, MI

260

Ward, Merrill, WI

100

Warren, Hinckley/Skowhegan, ME
Warren, Muskegon, MI
Warren, Westbrook, ME

Total 2535

Westvaco, Tyrone, PA

200

Westvaco, Wickliffe, KY

600

Weyerhaeuser, Longview, WA

360

Weyerhaeuser, Rothschild, WI

350

Whiting, Menasha, WI

25

 [Contents]  [Search]  [Abbey]


[Search all CoOL documents]


URL: http://www.cool.conservation-us.org/byorg/abbey/ap/ap03/ap03-1/ap03-116.html
Timestamp: Sunday, 03-Mar-2013 21:41:29 PST
Retrieved: Sunday, 21-Oct-2018 23:07:42 GMT


[Search all CoOL documents]


URL: http://www.cool.conservation-us.org/byorg/abbey/ap/ap03/ap03-1/ap03-116.html
Timestamp: Sunday, 03-Mar-2013 21:41:29 PST
Retrieved: Sunday, 21-Oct-2018 23:07:42 GMT