Alkaline Coated Freesheet

Many people believe that all lightweight coated paper (LWC) has a groundwood base sheet, and there are even some who believe that all coated paper is acidic or groundwood. It is true that most LWC has a lot of mechanical pulp in the base sheet, but there are quite a few coated papers, 45 lb. and up, that have alkaline freesheet base papers.

All of the papers listed below are identified in the Fine Paper Directory as having a pH over 7.5 and containing no groundwood. The names of the papers are actually the names of whole lines or families of papers.

Consolidated

Centura

Paloma

Consolith

Productolith

Frostbrite

Reflections

Glatfelter

Delcrest

Old Forge

Glatco

Velvetlith

James River

Capistrano II

Sonoma

Mead

Mead Mark

Signature from Mead

Mead Offset

 

Midtec, A Repap Enterprise

Excellence

Litho Web Plus

Midset

Lithofect Plus

Multiweb

 

Papyrus Newton Falls

NF Cote [Not in FPD]

St. Lawrence Offset

St. Lawrence Label

Stora Matte

Potlatch/Northwest

Eloquence

Northwest

Makers' Matte

Quintessence

Mountie

Vintage

Simpson

Solitaire

 

Warren

Cameo

Patina

Flokote

Somerset

Lusterkote ClS

Warrenflo

Lustro

Westvaco

Inspiration

Sterling

 

In Canada, Island Paper and Repap Enterprises are making alkaline coated freesheet.

 [Contents]  [Search]  [Abbey]


[Search all CoOL documents]


URL: http://www.cool.conservation-us.org/byorg/abbey/ap/ap03/ap03-2/ap03-212.html
Timestamp: Sunday, 03-Mar-2013 21:41:31 PST
Retrieved: Wednesday, 23-Jan-2019 17:38:15 GMT


[Search all CoOL documents]


URL: http://www.cool.conservation-us.org/byorg/abbey/ap/ap03/ap03-2/ap03-212.html
Timestamp: Sunday, 03-Mar-2013 21:41:31 PST
Retrieved: Wednesday, 23-Jan-2019 17:38:15 GMT