Company Capacity
(tons/day)
# Mills Making Fine Paper
Badger 1 375
Consolidated 1 1100
Cross Pointe 3 775
Eastern 1 200
E.B. Eddy 1 270
Esleek (N) 1 20
Finch Pruyn 1 600
Fletcher 1 85
Glatfelter (incl. Ecusta) 3 1215
Hammermill (exc. Strath) 5 2098
Lyons Falls 1 220
Millers Falls (div. of Strath) 1 50
Mohawk 2 230
Penntech (div. of Willamette) 400 Potlatch /Northwest 2 935
Potsdam 1 ?
Repap Wisconsin 1 1140
Riverside 1 120
Simpson Pasadena 1 750
Simpson Plainwell 1 260
Stora Papyrus Newton Falls 1 400
Ward (div. of Strathmore) 1 100
Weyerhaeuser 1 1850
Whiting, George A. 1 28
Willamette 2 1150

This table was compiled as an aid for people who are looking for alkaline paper, and need to know which companies they can buy from with confidence, i.e., which companies do not produce acidic printing or writing papers at all. The table has been maintained for several years in the Abbey Publications office, in hopes that one day it would be accurate enough to publish. It is probably as accurate now as it ever will be, though it is probably not perfect. It should be used with reasonable care.

One way to start a search for alkaline printing or writing paper is to look up nearby paper distributors in the Yellow Pages of the phone book.

 [Contents]  [Search]  [Abbey]


[Search all CoOL documents]


URL: http://www.cool.conservation-us.org/byorg/abbey/ap/ap06/ap06-3/ap06-310.html
Timestamp: Sunday, 03-Mar-2013 21:42:17 PST
Retrieved: Tuesday, 17-Jul-2018 19:08:31 GMT


[Search all CoOL documents]


URL: http://www.cool.conservation-us.org/byorg/abbey/ap/ap06/ap06-3/ap06-310.html
Timestamp: Sunday, 03-Mar-2013 21:42:17 PST
Retrieved: Tuesday, 17-Jul-2018 19:08:31 GMT